Products Description
SS 17-4PH is a stainless steel grade that belongs to the martensitic family and is hardened through precipitation. It consists of alloying elements such as nickel, copper, and chromium. This alloy is commonly used in the aerospace industry for applications such as fasteners and structural components.
The specific grade designation for SS 17-4PH is UNS S17400. The microstructure of this alloy is obtained through a remelting process, which results in a refined structure. This refined structure enhances the toughness of the alloy, making it more resistant to impact and mechanical stresses.
SS 17-4PH is a precipitation-hardening martensitic stainless steel grade. It contains alloying elements such as nickel, copper, and chromium. This alloy is frequently utilized in the aerospace industry for applications including fasteners and structural components.
The specific grade designation for SS 17-4PH is UNS S17400. The microstructure of this alloy is achieved through a remelting process, which leads to a refined structure. The refined structure contributes to increased toughness of the alloy, making it more resistant to impact and mechanical stresses.
17-4PH STAINLESS STEEL ROUND BAR EQUIVALENT GRADES
STANDARD |
UNS |
WNR. |
SS 17-4PH |
S17400 |
1.4542 |
CHEMICAL COMPOSITION OF STAINLESS STEEL 17-4PH ROUND BAR
Grade |
C |
P |
Si |
Ni |
Cu |
Fe |
Mn |
S |
Cr |
SS 17-4 PH |
0.07 max |
0.04 max |
1.0 max |
3.0 - 5.0 max |
3.0 - 5.0 max |
Bal |
1.0 max |
0.03 |
15.0 - 17.5 |
MECHANICAL PROPERTIES OF STAINLESS STEEL 17-4PH ROUND BAR
Tensile Strength |
Yield Strength (0.2%Offset) |
Elongation |
Rockwell Hardness |
160,000 |
145,000 |
5% |
C35 |
STANDARD |
UNS |
WNR. |
SS 17-4PH |
S17400 |
1.4542 |
Grade |
C |
P |
Si |
Ni |
Cu |
Fe |
Mn |
S |
Cr |
SS 17-4 PH |
0.07 max |
0.04 max |
1.0 max |
3.0 - 5.0 max |
3.0 - 5.0 max |
Bal |
1.0 max |
0.03 |
15.0 - 17.5 |
Tensile Strength |
Yield Strength (0.2%Offset) |
Elongation |
Rockwell Hardness |
160,000 |
145,000 |
5% |
C35 |